Preparation of Nylon 66

Preparation of Nylon 66 The polyamide Nylon 66 is formed by heating the reactant mixture under pressure and the process has been developed so that the molecular mass of the polymer is controlled in the range of 12,000 to 20,000 amu. Nylon-6 is prepared from the...